Magnetics Calculators29 instruments

B–H Hysteresis Loop

Animated loop, coercivity, remanence and energy per cycle.

w=∮H dBw=\oint H\,dB
Fig. 1 Live B–H loop: the red operating point is driven by a sinusoidal H(t)
-200-1000100200-101Bᵣ−HᴄH (A/m)B (T)
ascendingdescending
hover / touch plot to probe
Inputs drag, tap ± or type (SI suffixes ok: 4k7 → 4.7k)
T
T
A/m
Hz
kg/m³
Results
Loop area ∮H dB\oint H\,dB
287.4 J/m³
Hysteresis loss density
14.4 kW/m³1.879 W/kg
Peak BB reached
1.8 T
Loop coercivity / remanence
40 A/m / 1.2 T
Squareness Br/BsB_r/B_s
0.667
Steepest slope μr,max\mu_{r,max}
28,800
Magnetic class
soft

§ How it works

Ferromagnets remember: domain walls snag on defects, so the magnetisation lags the applied field and traces a loop. Key points are saturation BsB_s, remanence BrB_r (flux left at H=0H=0) and coercivity HcH_c (reverse field needed to bring BB to zero).

This tool uses a phenomenological tanh model, with branches shifted so the loop closes at the drive amplitude HmH_m:

B↑↓(H)=Bstanh⁡ ⁣(H∓Hch0)±Δ2+μ0H,h0=Hcartanh⁡(Br/Bs)B_{\uparrow\downarrow}(H) = B_s\tanh\!\left(\frac{H \mp H_c}{h_0}\right) \pm \frac{\Delta}{2} + \mu_0 H,\qquad h_0 = \frac{H_c}{\operatorname{artanh}(B_r/B_s)}

The energy dissipated per cycle and unit volume equals the enclosed area, w=∮H dBw = \oint H\,dB, computed numerically. Multiply by frequency for loss power: Pv=wfP_v = w f. Reducing the drive amplitude produces narrower minor loops: the reason Steinmetz's β\beta exponent exceeds 1.

Soft materials (transformer steel, ferrite, permalloy) have thin loops to minimise loss; hard materials (Alnico, NdFeB) have fat loops to retain magnetisation.